nav-butt

首页>Product >Failure analysis>Professional case analysis 4

Professional case analysis 4

Recommendations:

 

1. The original water inlet position is too small, so it is recommended to feed at the place with the red arrow;

 

2.Add slag at the position shown in the yellow box;

 

3.The spacing between cooling water holes is too large. It is recommended not to exceed  60-70 will be better.

 

The development and application of die casting mould steel is one of the main businesses of STRONG TECHNOLOGY company. Combined with Centennial Daye Special Steel and relying on the company's strong strength of material heat treatment for 30 years, it provides customers with one-stop solutions for die casting mould steel such as high-end high-quality base metal, machining, heat treatment, coating, mould design and maintenance and failure analysis.